Products<
D270 Injection Moulding Screw Barrel
產品介紹
Technical Information | |||
Main Base materials | 1.38CrMoAlA (SACM645) | Main Alloy Materials | 1. Ni-based alloy/Deloro alloy |
2. SKD-61 (Special Tool Steel) | 2. Tungsten carbide/Wolfram carbide | ||
3. 42CrMo (Ultrahigh StrengthSteel) | 3. NiCo-based alloy | ||
4. DC53 (Cold WorkDie Steel) | 4. Fe-based alloy | ||
5. W6Mo5Cr4V2 (High-SpeedToolSteel) | 5. Co-based alloy | ||
Processing Technics | 1. Heat treatment | Technical parameters | Nitriding layer depth:0.5-0.8mm |
2. Quenching | Nitrided hardness:900-1000HV | ||
3. Nitriding treatment | Bimetallic layer depth:3 mm | ||
4. Bimetallic alloy welding for screw | Bimetallic hardness:57~69HRC | ||
5. Bimetallic alloy centrifugal casting for barrel | Hard-chrome plating hardness after nitriding:≥950HV | ||
6. Hard-chrome electroplating | Chrome-plating layer depth:0.03-0.09mm | ||
Linearity of screw:0.015mm | Surface roughness:Ra 0.4 |
This parameter is based on our domestic machines and is just for your reference. If you have your own parameter, we can also make it.
Packaging Details
Injection molding screw barrel
1. Be brushed anti-corrosive oil on screw barrel.
2. Packed with film.